  1. This tester (Fig. 1) measures the energy required to puncture container board or corrugated board with a pyramidal point affixed to a pendulum arm. Results are reported in “puncture units,” comprised of two major components: the energy to tear the material and the energy to bend it out of the way of the point.

  2. 1 subscriber. 387 views 4 years ago. DESARROLLO DE PRUEBA DE PUNCION DEL CARTON CORRUGADO DE ACUERDO AL STD TAPPI T803.

  3. Applications. Tappi. TAPPI T 803 Puncture Test of Container Board. 0 0. Measures the energy required to puncture container board or corrugated board with a pyramidal point affixed to a pendulum arm. These energy units actually are made up of two major components: the energy to tear the material and the energy to bend it out of the way of the point.

  4. 1 de ene. de 2010 · This tester (Fig. 1) measures the energy required to puncture container board or corrugated board with a pyramidal point affixed to a pendulum arm. Results are reported in "puncture units," comprised of two major components: the energy to tear the material and the energy to bend it out of the way of the point.

  5. TAPPI T 803 om-20 Puncture test of container board. This tester (Fig. 1) measures the energy required to puncture container board or corrugated board with a pyramidal point affixed to a pendulum arm. These energy units actually are made up of two major components: the energy to tear the material and the energy to bend it out of the way of the ...

  6. The Puncture Tester measures the energy required to puncture container board or corrugated board with a pyramidal point… Contact Qualitest Phone: 1-877-884-8378

  7. 1 de ene. de 2020 · TAPPI T 803 – Puncture Test of Container Board. This tester (Fig. 1) measures the energy required to puncture container board or corrugated board with a pyramidal point affixed to a pendulum arm.